Çelik Boru Programları ve Boyutları

Oct 24, 2023

Çelik Boru Programları ve Boyutları

İnç
Not DN OD (İnç) Boru Programı
SCH 5 SCH 10 20 SCH 30 SCH 40 SCH SCH 60 80 SCH SCH 100 SCH 120 SCH 160
3/4 20 1.05 0.065 0.11 X 0.095 0.113 X X 0.17 X 0.219
1 25 1.315 0.065 0.11 X 0.114 0.133 X X 0.2 X 0.25
1 1/2 40 1.9 0.065 0.11 X 0.125 0.145 X X 0.225 X 0.281
2 50 2.375 0.065 0.12 X X 0.154 X X 0.25 X 0.344
2 1/2 65 2.875 0.083 0.12 X X 0.203 X X 0.3 X 0.375
3 80 3.5 0.083 0.12 X X 0.216 X X 0.35 X 0.438
4 100 4.5 0.083 0.12 X X 0.237 X X 0.437 X 0.531
5 125 5.563 0.109 0.12 X X 0.258 X X 0.5 X 0.625
6 150 6.625 0.109 0.13 X X 0.28 X X 0.562 X 0.719
8 200 8.625 0.109 0.15 0.25 0.277 0.322 0.406 0.5 0.593 0.719 0.906
10 250 10.75 0.134 0.17 0.25 0.307 0.365 0.5 0.594 0.718 0.843 1.125
12 300 12.75 0.156 0.18 0.25 0.33 0.406 0.562 0.687 0.843 1.0 1.312
14 350 14.0 0.156 0.25 0.312 0.375 0.437 0.593 0.75 0.937 1.093 1.406

Steel Pipe

Milimetre
Not DN Dış Çap (mm) Boru Programı
SCH 5 SCH 10 20 SCH 30 SCH 40 SCH SCH 60 80 SCH SCH 100 SCH 120 SCH 160
3/4 20 26.67 1.65 2.11 X 2.41 2.87 X 3.91 X 4.32 5.56
1 25 33.40 1.65 2.77 X 2.90 3.38 X 4.55 X 5.08 6.35
1 1/2 40 48.26 1.65 2.77 X 3.18 3.68 X 5.08 X 5.72 7.14
2 50 60.32 1.65 2.77 X X 3.91 X 5.54 X 6.35 8.74
2 1/2 65 73.02 2.11 3.05 X X 5.16 X 7.01 X 7.62 9.53
3 80 88.9 2.11 3.05 X X 5.49 X 7.62 X 8.89 11.13
4 100 114.3 2.11 3.05 X X 6.02 X 8.56 X 11.10 13.49
5 125 141.3 2.77 3.4 X X 6.55 X 9.53 X 12.70 15.88
6 150 168.27 2.77 3.4 X X 7.11 X 10.97 X 14.27 18.26
8 200 219.07 2.77 3.76 6.35 7.04 8.18 10.31 12.7 15.06 18.24 23.01
10 250 273.05 3.4 4.19 6.35 7.8 9.27 12.7 15.06 18.24 21.41 28.58
12 300 323.85 3.96 4.57 6.35 8.38 10.31 14.27 17.45 21.41 25.40 33.32
14 350 355.60 3.962 6.35 7.925 9.525 11.10 15.06 19.05 23.80 27.76 35.71

Steel Pipes