Paslanmaz Çelik Boru Boyut Tablosu
Oct 09, 2023
Paslanmaz Çelik Boru Boyut Tablosu
| TÜP DÇ (İNÇ) | BORU DIŞ ÇAPI (MM) | DUVAR KALINLIĞI (İNÇ) | DUVAR KALINLIĞI (MM) | BWG |
|---|---|---|---|---|
| 0.188 | 4.78 | 0.035 | 0.89 | 20 |
| 0.250 | 6.35 | 0.020 | 0.51 | |
| 0.028 | 0.71 | 22 | ||
| 0.035 | 0.89 | 20 | ||
| 0.049 | 1.25 | 18 | ||
| 0.065 | 1.65 | 16 | ||
| 0.313 | 7.95 | 0.035 | 0.89 | 20 |
| 0.049 | 1.25 | 18 | ||
| 0.375 | 9.53 | 0.028 | 0.71 | 22 |
| 0.035 | 0.89 | 20 | ||
| 0.049 | 1.25 | 18 | ||
| 0.065 | 1.65 | 16 | ||
| 0.500 | 12.7 | 0.035 | 0.89 | 20 |
| 0.049 | 1.25 | 18 | ||
| 0.650 | 1.65 | 16 | ||
| 0.625 | 15.88 | 0.035 | 0.89 | 20 |
| 0.049 | 1.25 | 18 | ||
| 0.065 | 1.65 | 16 | ||
| 0.750 | 19.05 | 0.035 | 0.89 | 20 |
| 0.049 | 1.25 | 18 | ||
| 0.065 | 1.65 | 16 | ||
| 0.083 | 2.11 | 14 | ||
| 0.120 | 3.05 | 11 | ||
| 0.875 | 22.23 | 0.035 | 0.89 | 20 |
| 0.049 | 1.25 | 18 | ||
| 0.065 | 1.65 | 16 | ||
| 0.120 | 3.05 | 11 | ||
| 1.000 | 25.4 | 0.035 | 0.89 | 20 |
| 0.049 | 1.25 | 18 | ||
| 0.065 | 1.65 | 16 | ||
| 0.083 | 2.11 | 14 | ||
| 0.095 | 2.41 | 13 | ||
| 0.120 | 3.05 | 11 | ||
| 1.125 | 28.58 | 0.065 | 1.65 | 16 |
| 1.250 | 31.75 | 0.065 | 1.65 | 16 |
| 0.083 | 2.11 | 14 | ||
| 0.120 | 3.05 | 11 | ||
| 1.375 | 34.93 | 0.035 | 0.89 | 20 |
| 1.5000 | 38.1 | 0.049 | 1.25 | 18 |
| 0.065 | 1.65 | 16 | ||
| 0.083 | 2.11 | 14 | ||
| 0.120 | 3.05 | 11 | ||
| 1.750 | 44.45 | 0.035 | 0.89 | 20 |
| 0.065 | 1.65 | 16 | ||
| 0.083 | 2.11 | 14 | ||
| 1.875 | 47.63 | 0.065 | 1.65 | 16 |
| 2.000 | 50.8 | 0.049 | 1.25 | 18 |
| 0.065 | 1.65 | 16 | ||
| 0.083 | 2.11 | 14 | ||
| 0.120 | 3.05 | 11 | ||
| 2.125 | 53.98 | 0.065 | 1.65 | 16 |
| 2.250 | 57.15 | 0.065 | 1.65 | 16 |
| 0.083 | 2.11 | 14 | ||
| 0.120 | 3.05 | 11 | ||
| 2.500 | 63.5 | 0.065 | 1.65 | 16 |
| 0.083 | 2.11 | 14 | ||
| 0.120 | 3.05 | 11 | ||
| 2.750 | 69.85 | 0.065 | 1.65 | 16 |
| 3.000 | 76.2 | 0.049 | 1.25 | 18 |
| 0.065 | 1.65 | 16 | ||
| 0.083 | 2.11 | 14 | ||
| 0.120 | 3.05 | 11 | ||
| 3.250 | 82.55 | 0.065 | 1.65 | 16 |
| 0.120 | 3.05 | 11 | ||
| 3.500 | 88.9 | 0.065 | 1.65 | 16 |
| 4.000 | 101.6 | 0.065 | 1.65 | 16 |
| 0.083 | 2.11 | 14 | ||
| 4.250 | 108 | 0.120 | 3.05 | 11 |
| 4.500 | 114.3 | 0.065 | 1.65 | 16 |
| 5.000 | 127 | 0.065 | 1.65 | 16 |
| 0.083 | 2.11 | 14 | ||
| 0.120 | 3.05 | 11 | ||
| 0.188 | 4.78 | |||
| 6.000 | 152.4 | 0.065 | 1.65 | 16 |
| 0.083 | 2.11 | 14 | ||
| 0.120 | 3.05 | 11 | ||
| 8.000 | 203.2 | 0.120 | 3.05 | 11 |